bolt
Thread tolerance: 6g
Model: M24X60
Standard type: German standard
ISBN: DIN933
Category: hexagon bolt
Surface treatment: without treatment
Brand: ZB/ bond
Scope of application: aviation special fasteners
Model: M24X60
Standard type: German standard
ISBN: DIN933
Category: hexagon bolt
Surface treatment: without treatment
Brand: ZB/ bond
Scope of application: aviation special fasteners